Current research projects

Image Preformance measurements of heat exchangers
Image Test rigs for refrigeration and heat pump technology
Image Calibration of Low Temperature Sensors
Image Reduction of primary noise sources of fans
Image Lifetime prediction of hermetic compressor systems
Image Investigation of coolants
Image Computational fluid dynamics CFD
Image Range of services laboratory analyses
Image In-situ investigation concerning the swelling behaviour of polymer materials under elevated pressures and temperatures
Image Test method for high - temperature heat pump - oils
Image Verification of storage suitability of cryo tubes
Image Cold meter
Image Measurement of insulated packaging
Image All-in-one device for freeze-drying and production of biomaterial
Image Software modules
Image ZeroHeatPump

You are here:   /  Home


Tensile and compression testing

Industry and research institutes

Gunar Schroeder

+49-351-4081-5129

Determination of yield strength, tensile strength and elongation at break

A tensile or compression test is a quasi-static, destructive test method for determining material characteristics such as yield strength, tensile strength and elongation at break. The specimen form and the procedure of such tests are standardized. The ISO 9862 standard defines the exact procedure and the measured variables to be recorded for metallic materials and the DIN 50125 standard defines the specimen shape and its production method. In addition, the arrangement can generally be used to record force-displacement curves with high accuracy.

To carry out the test, the specimens are clamped centrally in the grippers or positioned centrally between the compression plates. In the tensile test, the specimens are pulled apart in a defined manner. In the compression test, on the other hand, a compressive force is applied to the test specimen, e.g. rectangular prisms, cylinders or tubes, in a uniaxial stress state. In both tests, the force and change in length are recorded continuously and evaluated graphically. On request, the tensile and compression test can be carried out at very low temperatures.

Parameter Limit values samples
Materials foils, plastics, composites, metals
Typical dimension of plastic samples Lר: 200×10 mm (7.8"×0.4") or
L×W×H: 200×10×10 mm (7.8"×0.4"×0.4")
Measurement range of force and displacement ±5 kN (±1124 lbf), 400 mm (15.8")
Standardized testing force-distance, force-time, tension-extension

 


Your Request

Further Projects

Image

Ionocaloric cooling

Ionocaloric solid-liquid phase cooling process

Image

Low temperature – test facilities

thermal cycling tests at very low temperatures

Image

All-in-one device for freeze-drying and production of biomaterial

with automated freezing and sterilisation option