Current research projects

Image Reducing the filling quantity
Image In-situ investigation concerning the swelling behaviour of polymer materials under elevated pressures and temperatures
Image Energy efficiency consulting - cogeneration systems
Image Range of services laboratory analyses
Image Calibration of Low Temperature Sensors
Image Test method for high - temperature heat pump - oils
Image Innovative Parahydrogen Generator Based on Magnets
Image Low temperature – test facilities
Image Brine (water)-water heat pump
Image Humidifier System for High-Purity Gases
Image Non- invasive flow measurements
Image Performance tests of condensing units
Image Micro fluidic expansion valve
Image Electrochemical decontamination of electrically conducting surfaces „EDeKo II“
Image Optimizing HVAC operation with machine learning
Image Innovative Manufacturing Technologies for Cryosorption Systems

You are here:  Home /  Measurements and Tests


Tensile and compression testing

Industry and research institutes

Gunar Schroeder

+49-351-4081-5129

Determination of yield strength, tensile strength and elongation at break

A tensile or compression test is a quasi-static, destructive test method for determining material characteristics such as yield strength, tensile strength and elongation at break. The specimen form and the procedure of such tests are standardized. The ISO 9862 standard defines the exact procedure and the measured variables to be recorded for metallic materials and the DIN 50125 standard defines the specimen shape and its production method. In addition, the arrangement can generally be used to record force-displacement curves with high accuracy.

To carry out the test, the specimens are clamped centrally in the grippers or positioned centrally between the compression plates. In the tensile test, the specimens are pulled apart in a defined manner. In the compression test, on the other hand, a compressive force is applied to the test specimen, e.g. rectangular prisms, cylinders or tubes, in a uniaxial stress state. In both tests, the force and change in length are recorded continuously and evaluated graphically. On request, the tensile and compression test can be carried out at very low temperatures.

Parameter Limit values samples
Materials foils, plastics, composites, metals
Typical dimension of plastic samples Lר: 200×10 mm (7.8"×0.4") or
L×W×H: 200×10×10 mm (7.8"×0.4"×0.4")
Measurement range of force and displacement ±5 kN (±1124 lbf), 400 mm (15.8")
Standardized testing force-distance, force-time, tension-extension

 