Current research projects

Image High Capacity Pulse Tube Cooler
Image Filter Tests
Image Behavior of multiphase cryogenic fluids
Image Tribological investigations of oil-refrigerant-material-systems
Image Industry 4.0 membrane heat and mass exchanger (i-MWÜ4.0)
Image Performance tests of refrigerant compressors
Image All-in-one device for freeze-drying and production of biomaterial
Image Calibration leak for the water bath leak test
Image Innovative cryogenic cooling system for the recondensation / liquefaction of technical gases up to 77 K
Image Range of services laboratory analyses
Image Test rigs for refrigeration and heat pump technology
Image Software for technical building equipment
Image CO₂ GAS HYDRATES FOR SUSTAINABLE ENERGY AND COOLING SOLUTIONS
Image Cool Up
Image Energy efficiency consulting - cogeneration systems
Image Electrical components in refrigeration circuits

You are here:   /  Home


Tensile and compression testing

Industry and research institutes

Gunar Schroeder

+49-351-4081-5129

Determination of yield strength, tensile strength and elongation at break

A tensile or compression test is a quasi-static, destructive test method for determining material characteristics such as yield strength, tensile strength and elongation at break. The specimen form and the procedure of such tests are standardized. The ISO 9862 standard defines the exact procedure and the measured variables to be recorded for metallic materials and the DIN 50125 standard defines the specimen shape and its production method. In addition, the arrangement can generally be used to record force-displacement curves with high accuracy.

To carry out the test, the specimens are clamped centrally in the grippers or positioned centrally between the compression plates. In the tensile test, the specimens are pulled apart in a defined manner. In the compression test, on the other hand, a compressive force is applied to the test specimen, e.g. rectangular prisms, cylinders or tubes, in a uniaxial stress state. In both tests, the force and change in length are recorded continuously and evaluated graphically. On request, the tensile and compression test can be carried out at very low temperatures.

Parameter Limit values samples
Materials foils, plastics, composites, metals
Typical dimension of plastic samples Lר: 200×10 mm (7.8"×0.4") or
L×W×H: 200×10×10 mm (7.8"×0.4"×0.4")
Measurement range of force and displacement ±5 kN (±1124 lbf), 400 mm (15.8")
Standardized testing force-distance, force-time, tension-extension

 