Current research projects

Image Practical training, diploma, master, bachelor
Image Solar Cooling
Image Optimizing HVAC operation with machine learning
Image Helium extraction from natural gas
Image Low Temperature Measuring Service
Image Software for technical building equipment
Image Verification of storage suitability of cryo tubes
Image Characterisation of Superconductors in Hydrogen Atmosphere
Image Range of services laboratory analyses
Image Innovative cryogenic cooling system for the recondensation / liquefaction of technical gases up to 77 K
Image Investigation of material-dependent parameters
Image Cryostats, Non-Metallic and Metallic
Image Testzentrum PLWP at ILK Dresden
Image Innovative small helium liquefier
Image Low noise and non metallic liquid-helium cryostat
Image Ionocaloric cooling

You are here:  Home /  Research and Development


Investigation of material-dependent parameters

Industry and R&D

Gunar Schroeder

+49-351-4081-5129

Investigation of the permeation behavior

Permeation is the penetration of solid matter by another substance. The driving force for this is a gradient of the chemical potential of the permeate. In practice, this gradient is replaced by a measurable quantity such as the pressure gradient. The permeability of a material depends on the surface temperature and is usually specified with the unit \( \frac{\mu g}{cm^2\:min} \)

Without external influences, the permeate always moves in the direction of the lower concentration or the lower partial pressure. For theoretical consideration, permeation can be divided into three sections across the solid:

  • Sorption, for example, a gas is absorbed at the surface of the solid
  • Diffusion, this gas diffuses through the solid through molecular gaps towards the surface with a lower gas concentration
  • Desorption, the gas is released again from this surface

The experimental setup to investigate this process, see the following figures, essentially consists of a sample chamber. The sample is mounted with a seal or against a sealing surface. A test gas with a defined overpressure is applied to the volume on the "left" of the sample. The volume to the "right" of the sample is connected to a detector. The pressure on both sides of the sample, the temperatures and the gas flow rate are measured over a longer period of time (24 - 48 h).

Parameter Sample limits
materials plastics, metals
dimensions, diameter, and wall thickness 58 ... 60 mm, 1 ... 3 mm
other dimensions on request
pressure difference up to 10 bar (145 psi)
temperature range room temperature, other conditions on request
test gas helium or hydrogen
detector measuring range up to \(10^{-9} \frac{mbar\:l}{s} \), optional with calibration

 


Your Request

Further Projects - Research and Development

Image

State of system and failure analyses

Cause of the failure unknown?

Image

Thermostatic Expansion Valves

Does the TXV function correctly?

Image

Testzentrum PLWP at ILK Dresden

Test Fluid-Energy Machines and Components

Image

Performance tests of refrigerant compressors

Does your compressor perform well?

Image

Swirl-free on the move...

...with a contra-rotating fan